Abstract

The corrosion and electrochemical properties of three zinc single crystal surfaces with different orientations have been investigated. In near-neutral 1 M (NH4)2SO4, the corrosion rates on all three surfaces were found to be similar. However, the SEM morphologies of the corresponding corroded surfaces were markedly different from each other, but consistent with preferential attack of {1120} surfaces. In alkaline 0.5 N NaOH solution, the three sample orientations showed significantly different reactivities, with the (1120) surface exhibiting the highest reactivity and corrosion rate. Here, passivation ultimately occurred and the difference in the corrosion performance of the three surfaces, even for small overvoltages, is attributed to the presence of oxide or hydrated oxide films. © 1991.

Department(s)

Physics

Second Department

Materials Science and Engineering

International Standard Serial Number (ISSN)

0010-938X

Document Type

Article - Journal

Document Version

Citation

File Type

text

Language(s)

English

Rights

© 2023 Elsevier, All rights reserved.

Publication Date

01 Jan 1991

Share

 
COinS