Abstract
The linear and nonlinear low frequency internal friction of In-24 at. pct Tl displays a Curie-Weiss type behavior in the temperature range above the transformation temperature. The critical temperature equals the martensite start temperature. It is proposed that the origin of the observed internal friction is the diffusion-controlled interaction of substitutional atoms with the premartensitic strain modulation, tweed.
Recommended Citation
M. Wuttig et al., "PREMARTENSITIC ANELASTICITY IN INDIUM-THALLIUM ALLOYS.," Metallurgical transactions. A, Physical metallurgy and materials science, vol. 19 A, no. 4, pp. 789 - 792, Springer, Apr 1988.
The definitive version is available at https://doi.org/10.1007/bf02628358
Department(s)
Materials Science and Engineering
Second Department
Physics
International Standard Serial Number (ISSN)
0360-2133
Document Type
Article - Journal
Document Version
Citation
File Type
text
Language(s)
English
Rights
© 2023 Springer, All rights reserved.
Publication Date
01 Apr 1988