Abstract
WxSey thin films have been prepared by the spray pyrolysis and anodic electrodeposition of solutions of ammonium selenotungstate, (NH4)2WSe4, with y/x usually between two and three for the sprayed films and y x>>1 for the electrodeposited films. The sprayed films indicated regions of crystalline WSe2 and have optical absorbance spectra consistent with a mixture of WSe2, WSe3, and selenium. The electrodeposited films are totally amorphous, highly photoconductive, and have optical absorbance spectra typical of amorphous or vitreous selenium. The sprayed films transform into WO3 at temperatures greater than 350°C in the presence of oxygen wile the electrode-posited films tend to evaporate and/or decompose upon annealing. © 1985.
Recommended Citation
R. D. Engelken et al., "Growth Of Tungsten Selenide Films Through Pyrolytic Conversion And Anodic Electrooxidation Of Ammonium Selenotungstate ((NH4)2WSe4)," Materials Research Bulletin, vol. 20, no. 10, pp. 1173 - 1179, Elsevier, Jan 1985.
The definitive version is available at https://doi.org/10.1016/0025-5408(85)90091-1
Department(s)
Electrical and Computer Engineering
International Standard Serial Number (ISSN)
0025-5408
Document Type
Article - Journal
Document Version
Citation
File Type
text
Language(s)
English
Rights
© 2023 Elsevier, All rights reserved.
Publication Date
01 Jan 1985